| Specification |
Ampere Density: 15-24A/cm�;
Application Area: Steel Making;
Manufacturing Technique: Extruded Graphite;
Shape: Cylinder;
Grades: RP HP UHP Available;
Application 1: Electric Arc Furnace;
Application 2: Submerged Arc Furnace;
Nipple Type: Conical and Taper 4tpi;
Special Treatment: Anti-Oxidation Treatment;
Advantage: Low Consumption Rate;
Services: Engineers for Technical Supports;
Coefficient of Thermal Expansion: 2.3 Max;
Length: 1500~2700mm;
Resistivity: 5.0 Micro Ohm.M;
Flexural Strength: 10.5 MPa Min.;
Apply: Eaf, Submerged Arc Furnace, Ladle Furnace;
Diameter: 50~1200mm;
Picking: Wooden Box;
|
Ampere Density: 15-24A/cm�;
Application Area: Electrolysis;
Manufacturing Technique: Pressurized Vibration;
Shape: Trapezoid Type, Egg Type, Cylinder Type;
Si: Below0.28%;
P: Below0.004%;
V.M: 10-15%;
Ash: Below4.0%;
Fe: Below0.25%;
Resistivity: 65-90;
Density: Above1.46g/cm3;
Compression Strength: Above18MPa;
Real Density: Above1.98g/cm3;
|
Ampere Density: 15-24A/cm�;
Application Area: Electrolysis;
Manufacturing Technique: Pressurized Vibration;
Shape: Trapezoid Type, Egg Type, Cylinder Type;
Si: Below0.28%;
P: Below0.004%;
V.M: 10-15%;
Ash: Below4.0%;
Fe: Below0.25%;
Resistivity: 65-90;
Density: Above1.46g/cm3;
Compression Strength: Above18MPa;
Real Density: Above1.98g/cm3;
|
Ampere Density: 15-24A/cm�;
Application Area: Electrolysis;
Manufacturing Technique: Pressurized Vibration;
Shape: Trapezoid Type, Egg Type, Cylinder Type;
Si: Below0.28%;
P: Below0.004%;
V.M: 10-15%;
Ash: Below4.0%;
Fe: Below0.25%;
Resistivity: 65-90;
Density: Above1.46g/cm3;
Compression Strength: Above18MPa;
Real Density: Above1.98g/cm3;
|
Ampere Density: 15-24A/cm�;
Application Area: Electrolysis;
Manufacturing Technique: Pressurized Vibration;
Shape: Trapezoid Type, Egg Type, Cylinder Type;
Si: Below0.28%;
P: Below0.004%;
V.M: 10-15%;
Ash: Below4.0%;
Fe: Below0.25%;
Resistivity: 65-90;
Density: Above1.46g/cm3;
Compression Strength: Above18MPa;
Real Density: Above1.98g/cm3;
|